Compressive strength of concrete f'c= 210 kg/cm² with addition of 4%, 8% and 12% of diatomite and kaolin
DOI:
https://doi.org/10.18687/LACCEI2025.1.1.1515Palabras clave:
Concrete, diatomite, kaolin, compressive strength.Resumen
The purpose of this research is to determine the compressive strength of concrete f'c= 210 kg/cm² with addition of 4%, 8% and 12% of diatomite and kaolin; for this purpose, a quasi-experimental design of the applied type was applied considering a sample of 63 cylindrical concrete specimens; in which, 9 specimens belong to the standard concrete and 54 specimens to the concrete with addition of diatomite and kaolin in percentages of 4%, 8% and 12%. Likewise, the values obtained for the compressive strength of the standard concrete at 28 days of curing were 247.44 kg/cm² and of the concrete with addition of diatomite at 4%, 8% and 12% were 320.49 kg/cm², 180.32 kg/cm² and 117.46 kg/cm² respectively; however, the values of the concrete with addition of kaolin at 4%, 8% and 12% were 303.44 kg/cm², 299.65 kg/cm² and 247.91 kg/cm² respectively. Finally, it is concluded that concrete with diatomite addition at 4% increases the compressive strength of concrete by 29.52% with respect to the standard concrete; similarly, concrete with kaolin addition at 4%, 8% and 12% improves the compressive strength by 22.63%, 21.10% and 0.19%, respectively.Descargas
Publicado
2025-07-27
Número
Sección
Articles
Derechos de autor
Derechos de autor 2025 LACCEI
Licencia
Esta obra está bajo una Licencia Creative Commons Atribución-NoComercial-CompartirIgual 4.0 Internacional.
LACCEI conserva el copyright de todos los artículos publicados bajo los términos de su acuerdo de transferencia de copyright. Como titular del copyright, LACCEI distribuye los artículos al público bajo la Licencia Internacional Creative Commons Atribución-NoComercial-CompartirIgual 4.0 (CC BY-NC-SA 4.0).
Cómo citar
Tarrillo Portilla, E. I., & Velásquez Huayta, F. A. (2025). Compressive strength of concrete f’c= 210 kg/cm² with addition of 4%, 8% and 12% of diatomite and kaolin. LACCEI, 1(12). https://doi.org/10.18687/LACCEI2025.1.1.1515