Concrete of 210 kg/cm2 with Addition of Recycled Glass Before Pathogenic Agents

Autores/as

  • Villanueva Bazán, Henrry Josué
  • Gonzaga Toribio, Junior Jesús

DOI:

https://doi.org/10.18687/LACCEI2023.1.1.770

Palabras clave:

Recycled glass, Resistance fc=210 kg/cm2, sulfuric acid.

Resumen

This investigation was carried out with the purpose of analyzing the compressive strength of concrete f'c=210 kg/cm2 with recycled glass added in percentages of 5%, 10% and 15% and exposed to sulfuric acid during the process of cured. 108 test tubes were analyzed and applied in 4 groups of 27 according to control design, 5%, 10% and 15% Inclusion and exclusion techniques were used as the basis for this research. As data collection instruments, formats were used to support the tests carried out in the laboratory, in order to synthesize and organize the relevant information. Finally, the results of the resistance of the 108 test tubes were analyzed, concluding that the resistance increased according to the age of curing and the percentage added.

Descargas

Publicado

2023-07-27

Número

Sección

Articles

Licencia

Licencia Creative Commons

Esta obra está bajo una Licencia Creative Commons Atribución-NoComercial-CompartirIgual 4.0 Internacional.

LACCEI conserva el copyright de todos los artículos publicados bajo los términos de su acuerdo de transferencia de copyright. Como titular del copyright, LACCEI distribuye los artículos al público bajo la Licencia Internacional Creative Commons Atribución-NoComercial-CompartirIgual 4.0 (CC BY-NC-SA 4.0).

Cómo citar

Villanueva Bazán, Henrry Josué, & Gonzaga Toribio, Junior Jesús. (2023). Concrete of 210 kg/cm2 with Addition of Recycled Glass Before Pathogenic Agents. LACCEI, 1(8). https://doi.org/10.18687/LACCEI2023.1.1.770

Artículos más leídos del mismo autor/a