Influence of Thermal Waters Replacing 10%, 20% and 50% of Drinking Water on the Compressive Strength of Concrete

Authors

  • Simon Narva Guevara Universidad Privada del Norte - (PE), Perú
  • Eddson Mostacero Alva Universidad Privada del Norte - (PE), Perú

DOI:

https://doi.org/10.18687/LACCEI2026.1.1.1815

Keywords:

concrete, compressive strength, thermal waters.

Abstract

In construction, one of the most widely used materials is concrete due to its versatility, affordable cost, and durability. Its strength is fundamental and can be affected by the type, quantity, and quality of the water used. Freshwater resources are being depleted every day; therefore, alternative water sources are being considered, such as wastewater, seawater, rainwater, and thermal waters, among others. This thesis focuses on the influence of thermal waters as a partial replacement for potable water at percentages of 10%, 20%, and 50%, with the aim of analyzing their effect on the compressive strength of concrete designed for 210 kgf/cm2. Research shows that it is possible to use these types of water without adversely affecting the physical chemical strength of concrete. However, without treatment, thermal waters may affect the durability of concrete; for this reason, partial replacement of potable water is proposed. The key issue is to evaluate the chemical composition of the water before its use, since certain ions or solids may negatively affect the microstructure of concrete.

Downloads

Published

2026-07-27

License

Creative Commons License

This work is licensed under a Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International License.

LACCEI retains copyright of all published articles under the terms of its copyright transfer agreement. As the copyright holder, LACCEI distributes the articles to the public under the Creative Commons Attribution-NonCommercial-ShareAlike 4.0 International License (CC BY-NC-SA 4.0).

How to Cite

Narva Guevara, S., & Mostacero Alva, E. (2026). Influence of Thermal Waters Replacing 10%, 20% and 50% of Drinking Water on the Compressive Strength of Concrete. LACCEI, 1(14). https://doi.org/10.18687/LACCEI2026.1.1.1815